Superalloy Forgings
Superalloy forgings are a key component used in extreme environments such as high temperature, high pressure, and corrosion, and have important applications. High-temperature alloy forged are composed of nickel and copper with added elements such as aluminum and titanium, resulting in extremely high corrosion resistance and oxidation resistance.
Hastelloy grades are a group of corrosion-resistant alloys developed in harsh chemical environments. These grades exhibit superior mechanical strength and resistance to high temperatures and pressure extremes.
Furthermore, the unique composition of these grades allows them to be easily forged, making them an ideal choice for manufacturing equipment used in the chemical processing industry. The shapes of high-temperature alloy forging materials include sheets, plates, bars, and pipes, offering versatility in design options.
Email: [email protected]
WhatsApp: 0086-18301953841

| FORGING | TYPE | MAX. WEIGHT | MAX. DIMENSION | ALLOY | STANDARD |
| Open die forging | Cube | ≤ 15t | Length ≤ 7000mm , Width ≤ 1500mm , Height ≤ 800mm | A-286, HA188, Inconel 718, Inconel 600, Inconel X-750, Nimonic 90, Udimet 710, Incoloy 901, Incoloy 825, Hastelloy, Hastelloy X, Rene’41, Rene’95 | ASTM A837, ASTM B865, ASTM B637, AMS 5662, AMS 5666 |
| Disk | ≤ 10t | Diameter ≤ 2000mm | |||
| Ring / circle | ≤ 5t | Diameter ≤ 2500mm , Height ≤ 500mm | |||
| Cylinder | ≤ 5t | Diameter ≤ 1800mm , Length ≤ 1200mm | |||
| Axle | ≤ 15t | Length ≤ 7000mm , Diameter ≤ 800mm |
| ASTM | UNS | W-Nr. | JIS | KS | Element | DIN EN/DIN | ||||
| Incoloy800 | N08800 | 1.4876 | NCF800/2B | NCF800 | GH20 | 0Cr20Ni32AlTi | X10NiCrAlTi32-20 | |||
| Incoloy800H | N08810 | 1.4958 | NCF800H | 1Cr20Ni32AlTi | X10NiCrAlTi32-20 | |||||
| Incoloy800HT | N08811 | 1.4959 | 0Cr25Ni35AlTi | |||||||
| Incoloy825 | N08825 | 2.4858 | NCF825 | NCF825 | 0Cr21Ni42Mo3Cu2Ti | NiCr21Mo | ||||
| Incoloy901 | ||||||||||
| Incoloy925 | N09925 | |||||||||
| Incoloy926 | N08926 | 1.4529 | ||||||||
| Inconel600 | N06600 | 2.4816 | NCF1B | NCF600 | GH600 | 1Cr15Ni75Fe8 | NiCr15Fe8 | |||
| Inconel601 | N06601 | 2.4851 | NCF601 | NCF601 | 1Cr23Ni60Fe13Al | NiCr23Fe | ||||
| Inconel625 | N06625 | 2.4856 | NCF625 | NCF625 | 0Cr20Ni65Mo10Nb4 | NiCr22Mo9Nb | ||||
| Inconel690 | N06690 | 2.4642 | 0Cr30Ni60Fe10 | NiCr29Fe | ||||||
| Inconel718 | N07718 | 2.4668 | GH169 | NiCr19Fe19Nb5Mo3 | ||||||
| Inconel725 | N07725 | |||||||||
| Inconel X-750 | N07750 | 2.4669 | NCF750 | GH145 | XCr15Fe7TiAl | |||||
| HC-276 | N10276 | 2.4819 | 00Cr15Ni60Mo16W5Fe5 | NiMo15Cr15W | ||||||
| HB | N10001 | 2.4800* | 0Ni65Mo28Fe5V | S-NiMo 30 | ||||||
| HB-2 | N10665 | 3.4617 | 00Ni70Mo28 | NiMo28 | ||||||
| HB-3 | N10675 | 2.4600* | NiMo29Cr | |||||||
| HC | N10002 | 2.4819 | 0Cr15Ni60Mo16W5Fe5 | NiMo16Cr15W | ||||||
| HC-4 | N06455 | 2.4610* | 00Cr16Ni65Mo16Ti | NiMo16Cr16Ti | ||||||
| HC-22 | N06022 | 2.4602 | NiMo21Cr14W | |||||||
| HC-2000 | N06200 | 2.4675 | NiCr23Mo16Cu | |||||||
| Hastelloy-X | N06002 | 2.4465 | ||||||||
| Monel400 | N04400 | 2.4360,2.4361 | ||||||||
| MonelK500 | N05500 | 2.4375 | ||||||||
| Monel401 | N04401 | |||||||||
| Monel404 | 2.4867 | |||||||||
| Ni 200 | N02200 | 2.4066 | ||||||||
| Ni 201 | N02201 | |||||||||
| Nitronic50 | S20910 | XM-19 | ||||||||
| Nitronic60 | S21800 | Alloy218 | ||||||||
| Alloy20 Cb-3 | N08020 | 2.4660* | Carpeter20Cb-3 | 0Cr20Ni35Mo3Cu4Nb | NiCr20CuMo | |||||
| Alloy31 | N08031 | 1.4562 | X1NiCrMoCu 32-28-7 | |||||||
| Alloy33 | N08033 | 1.4591 | X1NiCrMoCuN 33-32-1 | |||||||
| ASTM | UNS | W-Nr. | JIS | KS | Element | DIN EN/DIN | ||||
| Alloy20 Cb-3 | N08020 | 2.4660* | Carpeter20Cb-3 | 0Cr20Ni35Mo3Cu4Nb | NiCr20CuMo | |||||
| IncoloyA-286 | S66286 | 1.4980,1.4944 | SUH660 | |||||||
| Incoloy800 | NO8800 | 1.4876 | NCF800B | NCF2B | GH20 | 0Cr20Ni32AlTi | X2NiCrAlTi3220 | |||
| Nimonic75 | 2.4951 | |||||||||
| N06219 | 2.4855 | NiCr19Mo9Si | ||||||||
| HastelloyX | N06002 | 2.4613 | ||||||||
| Inconel600 | N06600 | 2.4816 | NCF1B | NCF600 | GH600 | 1Cr15Ni75Fe8 | NiCr15Fe8 | |||
| Inconel625 | N06625 | 2.4856 | NCF625 | NCF625 | NS3306 | 0Cr20Ni65Mo10Nb4 | NiCr22Mo9Nb | |||
| InconelX-750 | N07750 | 2.4669 | NCF750 | XCr15Fe7TiAl | ||||||
| Nimonic80A | N07080 | 2.4952 | ||||||||
| Inconel718 | N07718 | 2.4668 | GH4169 | |||||||
| Inconel725 | N07725 | |||||||||
| Incoloy925 | N09925 | |||||||||
| Inconel600 | N06600 | 2.4816 | NCF600 | NCF1B | 1Cr15Ni75Fe8 | LC-NiCr15Fe | ||||
| PB | ||||||||||
| Alloy4 | ||||||||||
| Alloy31 | N08031 | 1.4562 | ||||||||
| F15 | ||||||||||
| Invar36 | K93600 | 1.3912 | ||||||||



We also provide CNC precision machining services for our clients, covering industries such as energy, petrochemicals, steel, engineering machinery, plastics, prevention and control, hydraulics, healthcare, and food. Please feel free to send us drawings for inquiries.